Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C
Subcategory: Stainless Steel; Metal
Key Words: UNS N08026, Carpenter Technology Corporation, Carpenter Steel Division; Cartech
Material Notes: Iron content calculated as remainder. Data provided by Carpenter Technology Corporation. This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, crevice corrosion and stress-corrosion cracking in chloride environments and is also resistant to oxidizing media. The alloy is designed for applications where better pitting and crevice-corrosion resistance are requires than 20Cb-3® stainless offers. 20-Mo6® is a registered trademark of Carpenter Technology Corporation.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|