Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 149°C (300°F)

 

Subcategory: Stainless Steel; Metal

Key Words: UNS N08026, Carpenter Technology Corporation, Carpenter Steel Division; Cartech

Material Notes:
Iron content calculated as remainder. Data provided by Carpenter Technology Corporation.

This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, crevice corrosion and stress-corrosion cracking in chloride environments and is also resistant to oxidizing media. The alloy is designed for applications where better pitting and crevice-corrosion resistance are requires than 20Cb-3® stainless offers.

20-Mo6® is a registered trademark of Carpenter Technology Corporation.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。