Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 468°C
Subcategory: Tool Steel; Air-Hardening Steel; Metal
Key Words: UNS K92580, Carpenter Technology Corporation, Carpenter Steel Division; Cartech
Material Notes: Iron content calculated as remainder. Data provided by Carpenter Technology Corporation. This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for components which require a combination of HRC 53/55 hardness with the highest toughness available. AerMet® is a registered trademark of Carpenter Technology Corporation.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Charpy Impact
- Shear Strength
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|