Carpenter AerMet 310
Subcategory: Tool Steel; Alloy Steel; Metal
Material Notes: AerMet 310 alloy possesses higher hardness and strength than AerMet 100 alloy while maintaining exceptional ductility and toughness. At a 310 ksi (2137 MPa) ultimate tensile strength, AerMet 310 alloy exhibits toughness values equivalent to alloys 20 ksi (138 MPa) lower in strength. The alloy should be considered as a candidate for use in components requiring high strength, high fracture toughness and exceptional resistance to stress corrosion cracking and fatigue.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Yield Strength
- Elongation at Break
- Reduction of Area
- Tensile Modulus
- Charpy Impact
- Fatigue Strength
- Fracture Toughness
|
|
|
|