Carlson Alloy 303 Austenitic Stainless Steel

 

Subcategory: Stainless Steel; Alloy Steel; Metal; Austenitic

Key Words: UNS S30300

Material Notes:
Carlson 303 is an austenitic free-machining stainless steel. The standard 18-8 stainless steels are more difficult to turn, mill and drill which restricts their use when considerable machining is required. The additional sulfur present in 303 assists in breaking up turnings which reduces drag on the cutting tool. This permits greater machining speed and tends to produce smoother machined finishes which in turn lowers production costs.

This material is not as resistant to general corrosion as is 304. It tends to form a rust film more readily in moist atmospheres and is very susceptible to pitting or localized corrosion in solutions of chlorides, iodides, or bromides. Under relatively dry conditions or in mildly corrosive environments, 303 resists rust. It also has good resistance to oxidation up to 1700°F. 303 is not recommended for vessels containing gases or liquids under high pressure. It is available as hot rolled, annealed and pickled (HRAP) or hot rolled, annealed only (HRA) plate.

Applications

Carlson 303 is utilized wherever a combination of good corrosion resistance and considerable machining is required for a part. Applications include aircraft fittings, computer motor holder rings, bushings, fittings, pump and valve parts, screw machine products, shafts and other parts requiring extensive machining.

Information provided by Carlson

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Reduction of Area
  • Electrical Resistivity
  • CTE, linear 68°F
  • Specific Heat Capacity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。