Carlson Alloy 303 Austenitic Stainless Steel
Subcategory: Stainless Steel; Alloy Steel; Metal; Austenitic
Key Words: UNS S30300
Material Notes: Carlson 303 is an austenitic free-machining stainless steel. The standard 18-8 stainless steels are more difficult to turn, mill and drill which restricts their use when considerable machining is required. The additional sulfur present in 303 assists in breaking up turnings which reduces drag on the cutting tool. This permits greater machining speed and tends to produce smoother machined finishes which in turn lowers production costs.This material is not as resistant to general corrosion as is 304. It tends to form a rust film more readily in moist atmospheres and is very susceptible to pitting or localized corrosion in solutions of chlorides, iodides, or bromides. Under relatively dry conditions or in mildly corrosive environments, 303 resists rust. It also has good resistance to oxidation up to 1700°F. 303 is not recommended for vessels containing gases or liquids under high pressure. It is available as hot rolled, annealed and pickled (HRAP) or hot rolled, annealed only (HRA) plate. Applications Carlson 303 is utilized wherever a combination of good corrosion resistance and considerable machining is required for a part. Applications include aircraft fittings, computer motor holder rings, bushings, fittings, pump and valve parts, screw machine products, shafts and other parts requiring extensive machining. Information provided by Carlson
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Yield
- Reduction of Area
- Electrical Resistivity
- CTE, linear 68°F
- Specific Heat Capacity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|