Carlson Alloy 2205 (UNS S32205) Duplex Stainless Steel

 

Subcategory: Stainless Steel; Alloy Steel; Metal; Austenitic; Duplex

Key Words: UNS S32205

Material Notes:
General Description

Carlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resistance over a wide range of applications. The approximate 50/50 ferrite-austenite structure provides excellent chloride pitting and stress corrosion cracking resistance, with roughly twice the yield strength of the standard austenitic stainless grades.

The high chromium and molybdenum content, coupled with the nitrogen addition in 2205, provides general corrosion, pitting, and crevice corrosion resistance superior to 316L and 317L.

2205 demonstrates superior erosion-corrosion resistance when compared to 316 stainless steel. It is not subject to intergranular corrosion in the as-welded condition. 2205 may be successfully machined by conventional methods.

The (UNS S32205) grade is a restricted-chemistry version which maintains chromium, molybdenum and nitrogen at higher levels than the (UNS S31803) composition.

Applications

Due to its excellent corrosion resistance, 2205 is a suitable material for service in environments containing chlorides and hydrogen sulfide. It is also suitable foe use in dilute sulfuric acid solutions and for handling organic acids, i.e., acetic acid and its mixtures.

  • Oil and Gas Production – Down-hole piping, gathering line pipe, CO2 tertiary recovery piping, oil-gas separators, heat exchangers.
  • Chemical Processing – Heat exchangers, pressure vessels, tanks, columns, pumps, valves, piping.
  • Transportation – Tank trailers, ocean-going tankers, barges.
  • Pulp & Paper – Pulp digesters
  • Power Industry – Feedwater heaters, coolers, flue gas scrubbers.
  • Marine Service – Sea water piping, pumps.

Information provided by Carlson

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • CTE, linear 68°F
  • Specific Heat Capacity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。