Carlson Alloy 330 Austenitic Alloy

 

Subcategory: Nickel Alloy; Metal; Austenitic

Key Words: UNS N08330

Material Notes:
General Description

Carlson Alloy 330 is a nickel-iron-chromium-silicon austenitic alloy. It combines high strength with excellent resistance to carburization and oxidation at temperatures to 2200°F (1200°C).

330 remains completely austenitic at all temperatures; and is totally immune to sigma phase formations.

With a 34 to 37 percent nickel content, 330 is highly resistant to chloride stress corrosion cracking. This high temperature alloy is often utilized for applications where conventional austenitic stainless steels are marginal.

Applications

330 is used extensively in elevated temperature environments where resistance to the combined effects of thermal cycling and carburization is required.

  • Furnace Containers – annealing, carbonitriding, malleablizing.
  • Heat Treating Equipment – muffles, retorts, conveyor systems, baskets, boxes, quenching fixtures.
  • Gas Turbine Components
  • Heat Exchangers
  • Furnace Fans
  • Petrochemical Furnace Parts
  • Salt Pots – neutral, cyanide
  • Hot Pressing Platens.

Information provided by Carlson

Available Properties
  • Density
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Magnetic Permeability
  • CTE, linear 68°F
  • Specific Heat Capacity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。