Carlson Alloy C 20 Plus Austenitic Alloy
Subcategory: Nickel Alloy; Metal; Austenitic
Key Words: UNS N08020
Material Notes:
Carlson C20 Plus is a super-austenitic alloy, developed to provide maximum resistance to corrosion by sulfuric acid. Nickel chromium, molybdenum and copper contribute to the excellent overall resistance of C 20 Plus to chloride stress corrosion cracking and general pitting. Because this alloy is stabilized with columbium, it can be used in the as-welded condition, thus expediting on-site fabrication. Applications Although C 20 Plus was developed primarily for sulfuric acid applications, it is also widely used in other chemical processing environments. C 20 Plus is employed in flue-gas scrubbers, sulfuric acid pickling, and in various other industries such as petroleum refining, pulp and paper, food and dyes. - Chemical Processing – sulfuric acid, phosphoric acid, pesticides, formic and nitric acids, butadiene (synthetic rubber), caustics, solvents, explosives.
- Petroleum Refining.
- Flue Gas Scrubbing Systems
- Pulp and Paper
- Food and Dye Processing
- Sulfuric Acid Pickling Equipment.
Information provided by Carlson
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Yield
- Modulus of Elasticity
- CTE, linear 68°F
- Specific Heat Capacity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|