Carlson Alloy C 601 Nickel-Chromium-Iron Alloy

 

Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal

Key Words: UNS N06601

Material Notes:
General Description

Carlson Alloy C 6021 is a nickel-chromium alloy, developed specifically for high –temperature service. This alloy exhibits outstanding resistance to both cyclic and static oxidation at temperatures up to 2300°F (1260°C). It has good resistance to aqueous corrosion and high mechanical strength.

The high chromium and nickel content of C 601 provide a substantial degree of resistance to carburizing, nitriding and sulfur containing environments. The nickel-base also assures good resistance to stress corrosion cracking.

C 601 exhibits excellent tensile and yield strengths and good creep-rupture strength. It will not become embrittled by extended exposure to high temperatures.

Applications

  • Thermal Processing – baskets, trays and fixtures for annealing, carburizing, carbonitriding, nitriding and other heat treating applications: radiant tubes, muffles, retorts, flame shields and burner nozzles in industrial furnaces; furnace atmosphere generators; infrared radiant shields.
  • Chemical Processing – process heaters and insulating cans in ammonia reformers; combustion components and catalyst grid supports in nitric acid production; catalyst regenerators and air preheaters in polyethylene production.
  • Pollution Control – combustion chambers in solid waste incinerators
  • Power Generation – superheater tube supports, grid barriers and ash-handling systems.
  • Gas Turbines – containment rings

Information provided by Carlson

Available Properties
  • Density
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Creep Strength
  • Modulus of Elasticity
  • Poissons Ratio
  • Electrical Resistivity
  • Curie Temperature
  • CTE, linear 68°F
  • Specific Heat Capacity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。