Carlson Alloy 70 30 Cu Ni Copper-Nickel Alloy
Subcategory: Copper Alloy; Nickel Alloy; Nonferrous Metal
Key Words: UNS C71500
Material Notes: General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temperatures and pressures, combined with high velocities and turbulence are serious problems. It can be utilized up to 700°F for ASME code heat exchangers and unfired pressure vessels. 70 30 Cu Ni exhibits outstanding resistance to general and impingent attack by clean sea water. It is, however, subject to bio-fouling at low velocities. 70 30 Cu Ni also has excellent resistance to attack by fresh water, boiler feedwater, and steam. It withstands the attack of phosphoric, sulfuric, and mild organic acids. It is attacked by chromic, hydrobromic, hydrochloric, and nitric acids. 70 30 Cu Ni is resistant to alkaline chlorides, chromates, nitrates and sulfates. It is, however, attacked by the cyanides and acid dichromates. 70 30 Cu Ni resists wet and dry chlorine, bromine, and carbon dioxide at ambient temperatures. Applications 70 30 Cu Ni is widely used in marine service, tidewater power plants, desalinization plants, oil refineries, and in the chemical process industry. It is utilized extensively as a condenser and salt water tube and piping material for the U.S. Navy. Product applications include condenser, heat exchanger and distiller tubes, tube sheets and baffles, sale water piping, water boxes, tanks, vats, pressure vessels, process equipment, pumps and valves. Information provided by Carlson
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Yield
- Modulus of Elasticity
- CTE, linear 68°F
- Specific Heat Capacity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|