Carlson Alloy 90 10 Cu Ni Copper-Nickel Alloy

 

Subcategory: Copper Alloy; Nickel Alloy; Nonferrous Metal

Key Words: UNS C70600

Material Notes:
General Description

Carlson Alloy 90 10 Cu Ni is a copper-based alloy developed as a cost-effective substitute for 70 30 Cu Ni. An addition of approximately 1.4% iron was made to increase its resistance to general corrosion, erosion and impingement corrosion resulting form the turbulent flow of water containing air bubbles and silt flowing at a high velocity. 90 10 Cu Ni has good strength at moderately elevated temperatures. It can be fabricated by both hot and cold-working procedures, and is readily weldable.

90 10 Cu Ni has excellent resistance to corrosion by fresh water, brackish water, and sea water. It is not recommended for usage in heavily polluted water containing sewage and industrial wastes. 90 10 Cu Ni resists attack by phosphoric, sulfuric, and mild organic acids. It is attacked by chromic, hydrochloric and nitric acids. 90 10 Cu Ni is also resistant to the alkali chlorides, nitrates, sulfates and to ammonia and ammonium compounds.

Applications

90 10 Cu Ni is widely used in marine service, offshore platform sea water piping, tidewater power plants, desalination plants, oil refineries, and in the chemical process industry.

Product applications include condenser tubes and plates, distiller tubes, tube sheets and baffles for condensers and heat exchangers, evaporator and heat exchanger tubes, salt water piping, water boxes, ship hulls and hot water tanks.

Information provided by Carlson

Available Properties
  • Density
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • CTE, linear 68°F
  • Specific Heat Capacity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。