Carpenter Extendo-Die® Hot Work Die Steel, Tempered 560°C
Subcategory: Tool Steel; Air-Hardening Steel; Hot Work Steel; Metal
Key Words: UNS K92580, Carpenter Technology Corporation, Carpenter Steel Division; Cartech
Material Notes: Iron content calculated as remainder. Data provided by Carpenter Technology Corporation. This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applications where H13 is currently used, particularly in large section size applications. Extendo-Die® hot work die steel can be water cooled in service. Extendo-Die® is a registered trademark of Carpenter Technology Corporation.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- CTE, linear 20°C
- CTE, linear 500°C
- Transformation Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|