Carpenter Micro-Melt® M-4 Alloy (AISI M4)

 

Subcategory: Tool Steel; Tungsten Alloy; High Carbon Steel; Metal

Key Words: UNS T11304

Material Notes:
Description: Micro-Melt® T-15 alloy is a high-carbon tungsten-cobalt-vanadium high speed powder metal. This grade possesses very high wear resistance coupled with high strength. The advantages of Micro-Melt premium powder high speed steels include ease of grinding, response to heat treatment, more uniform structure, greater wear resistance and improved toughness. In addition, Carpenter's unique hot rolling and rotary forging capabilities impart minimal distortion characteristics to these alloys. Micro-Melt M-4 alloy changes size only slightly after hardening. A 1" cube will expand about 0.0005" in hardening at 2225°F and will expand a like amount when tempered at 1050°F. Iron calculated as balance.

Applications: Lathe tools, Planer tools, Drills, Taps, Reamers, Broaches, Milling cutters, Form cutters, Thread chasers, Hobs, Counterbores, Inserts-heading dies

Information provided by Carpenter Technology Corporation.

Available Properties
  • Specific Gravity
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • CTE, linear 20°C
  • CTE, linear 500°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。