Carpenter Pyrotough® 78 Hot Work Die Steel

 

Subcategory: Tool Steel; Carbon Steel; Hot Work Steel; Metal

Material Notes:
Description: Pyrotough® 78 alloy is a premium quality hot work die steel engineered to withstand the operating temperatures and pressures associated with die casting and hot extrusion operations. The patented composition of the alloy displays improved temper resistance/red-hardness and similar toughness when compared to standard AISI type H13 hot work die steel. Careful control over all stages of processing results in an alloy possessing a high degree of purity, homogeneity and microstructural integrity. Iron calculated as balance.

Applications: mandrels for extruding copper, brass, stainless steel, and nickel-base superalloys, dies for extruding copper and brass

Information provided by Carpenter Technology Corporation.

Available Properties
  • Specific Gravity
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Yield
  • Reduction of Area
  • Charpy Impact
  • Abrasion
  • CTE, linear 20°C
  • Transformation Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。