Ceradyne Semicon SEMICORE® S2-17A MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet
Subcategory: Electronic/Magnetic Alloy; Cobalt Alloy
Material Notes: Magnetic alignment at 90° to Compaction AxisApplications: Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft sealsLightweight generators, usually for aircraftVane actuators for missiles Particle beam focusing, quadrupoles, lenses, wigglers, etc.Magnetic bearings, gyros, vacuum pumps, accelerometers Various mechanisms in disk drives, cameras, tape drives, and miniature loudspeakers and earphones; where small size is important Magnetic alignment at 90° to compaction angle. Information provided by Ceradyne Company
| Available Properties |
- Density
- Electrical Resistivity
- Magnetic Coercive Force, Hc
- Magnetic Remanence, Br
- Magnetic Maximum Energy Product, BH
- Curie Temperature
- CTE, linear 20°C
- Thermal Conductivity
- Room Temperature Compensation, RTC, %/°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|