CMW® 3970 (AMS-T-21014 ASTM B777) High Density Machinable Tungsten
Subcategory: Tungsten Alloy; Nonferrous Metal; Refractory Metal
Material Notes: Uses: Radiation Shielding, High Mass, Gyro, Ordnance Information provided by CMW Inc.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |