CMW ELKALOY® D Copper Alloy, Aluminum Bronze

 

Subcategory: Copper Alloy; Nonferrous Metal; Bronze

Material Notes:
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and thermal conductivity and ductility. In the ELKALOY® D alloy impurities (including iron) are kept low to obtain maximum electrical thermal conductivity.

ELKALOY® D material is recommended for certain flash welding operations, particularly for cold rolled steel and stainless set. The entire die is made from ELKALOY® D material. ELKALOY® D material is also used as a backing on barrel welding dies, faced with either CMW® 73 or ELKONITE® materials. The material may be used as an inexpensive current carrying member for welders or welding jigs, fixtures, or dies where high electrical conductivity is not of prime importance. Typical examples of welder arms, knees, platens and die and fixture bases.

Information provided by CMW Inc.

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear 100°C
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。