CMW® D50F Silver Nickel Alloy

 

Subcategory: Silver Alloy; Precious Metal; Nonferrous Metal

Material Notes:
CMW® D50F can be fabricated into wire, rod and strip; however, the headability of CMW® D50F is limited to a narrow range. It is used for main contacts in circuit breakers and switching devices where auxiliary contacts are used. This type of material has good resistance to mechanical wear under high contact forces, and maintains a stable surface resistance.

Information provided by CMW Inc.

Available Properties
  • Density
  • Hardness, Rockwell F
  • Tensile Strength, Ultimate
  • Electrical Resistivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。