CMW ELKONIUM® 1 silver, copper, nickel alloy

 

Subcategory: Silver Alloy; Precious Metal; Nonferrous Metal

Material Notes:
Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the alloys retain good current switching characteristics. Corrosion resistance decreases as the copper content increases. Copper oxides and other films will increase the surface resistance of these materials. This will require higher closing forces, usually 2 ounces or more, and some wiping action to break through the films and establish good contact. Because of the oxidation tendency, the silver-copper alloys should be avoided in high temperature applications. The silver-copper alloy materials are ductile and can be made in almost all the same shape and size contacts as fine silver. Usually, they will show an economical advantage over fine silver.

COIL SILVER AND ELKONIUM® 1 alloys are the most widely used materials of this group for electrical contacts. ELKONIUM® 1 material sold by CMW displays low transfer tendencies and high current switching capability in a number of automotive applications. Coin silver also has been used in a number of relays and switches because it is more economical than fine silver. It has been used in rotary switches and other sliding contact applications because it has good resistance to mechanical wear. Both coil silver and ELKONIUM 1 materials are used in high contact force applications where fine silver has failed by mechanical wear or deformation due to its lower hardness.

Information provided by CMW Inc.

Available Properties
  • Density
  • Hardness, Rockwell 15T
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Electrical Resistivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。