CMW ELKONIUM® 18 silver, copper, cadmium alloy
Subcategory: Silver Alloy; Precious Metal; Nonferrous Metal
Material Notes: The alloying of silver with cadmium produces materials with good arc extinction, good corrosion resistance and low contact resistance characteristics and provides them with good switching capability in AC circuits. They have low transfer characteristics in some DC applications. The alloying increases the strength and hardness, but substantially reduces the thermal and electrical conductivity and thus limits their current handling capability.
The silver-cadmium alloy contacts are ductile materials and can be supplied in shapes and sizes similar to fine silver. ELKONIUM® 18 alloy, in the spring temper condition, has a proportional limit of 33,000 psi, a modulus of elasticity of 10 X 106 psi, good corrosion resistance and is frequently used as a current carrying spring contact. Information provided by CMW Inc.
| Available Properties |
- Density
- Hardness, Rockwell 15T
- Tensile Strength, Ultimate
- Elongation at Break
- Electrical Resistivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|