CMW ELKONIUM® 22 silver, copper alloy
Subcategory: Silver Alloy; Precious Metal; Nonferrous Metal
Material Notes: Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the alloys retain good current switching characteristics. Corrosion resistance decreases as the copper content increases. Copper oxides and other films will increase the surface resistance of these materials. This will require higher closing forces, usually 2 ounces or more, and some wiping action to break through the films and establish good contact. Because of the oxidation tendency, the silver-copper alloys should be avoided in high temperature applications.
The silver-copper alloy materials are ductile and can be made in almost all the same shape and size contacts as fine silver. Usually, they will show an economical advantage over fine silver. ELKONIUM 22, the eutectic alloy, contains the highest amount of copper, which will give acceptable contact performance. It has higher contact resistance and greater sticking tendencies than CMW's ELKONIUM 1 alloy. Information provided by CMW Inc.
| Available Properties |
- Density
- Hardness, Rockwell 15T
- Tensile Strength, Ultimate
- Elongation at Break
- Electrical Resistivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|