CMW ELKONIUM® 36 Silver Alloy

 

Subcategory: Silver Alloy; Precious Metal; Nonferrous Metal

Material Notes:
The alloying of small amounts of one of the precious metals, platinum, palladium or gold with silver increases the hardness, and reduces the metal transfer tendency. These alloys maintain a low contact resistance during operation, as they are not susceptible to oxidation. They are susceptible to sulfide tarnishing however, to about the same degree as fine silver. They are suitable for contacts in sensitive devices in both AC and DC circuits.

ELKONIUM® 36, a silver platinum alloy, and ELKONIUM® 45, a silver palladium alloy, both have low contact resistance comparable to fine silver. They are used in DC applications where contact forces are low and fine silver transfers excessively. ELKONIUM® 45 alloy is employed as a negative contact operating against a positive contact material such as ELKONIUM® 17, CMW® D55X (silver-cadmium oxide) or CMW® D510 (silver-nickel) alloys. These combinations are used in low voltage DC applications such as vibrating contact voltage regulators to minimize metal transfer.

Information provided by CMW Inc.

Available Properties
  • Density
  • Hardness, Rockwell 15T
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Electrical Resistivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。