CMW ELKONIUM® 73 Copper Cadmium Alloy with Au/Ag-Cladding
Subcategory: Silver Alloy; Precious Metal; Nonferrous Metal
Material Notes: ELKONIUM 73 alloy is a silver, copper, cadmium and gold material marketed by CMW with high electrical and thermal properties. It is designed as an economical rivet type contact for AC applications requiring a moderate switching life at low to medium currents, as in appliance switches and control devices. Information provided by CMW Inc.
| Available Properties |
- Density
- Hardness, Rockwell 15T
- Tensile Strength, Ultimate
- Elongation at Break
- Electrical Resistivity
|
|
|
|