CMW ELKONIUM® 34 platinum based alloy

 

Subcategory: Precious Metal; Nonferrous Metal; Platinum Alloy

Material Notes:
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (1769(C) and good resistance to forming arcs. Low electrical conductivity (15% IACS) limits its application to low currents, usually below 5 amperes. Because of the high cost of the platinum ELKONIUM alloys, they are almost always supplied as composite contacts with thin facings of the ELKONIUM metal (silver brazed to nickel plated steel backings in the form of rivets, screws and weld buttons).

ELKONIUM 34, ELKONIUM 305 and ELKONIUM 306 alloys have lower ruthenium contents and are softer and more ductile. They can be headed into rivets over a limited range. All five alloys have low transfer characteristics and are used in voltage regulators and motor speed governors. They can be used as a positive contact paired with tungsten negative contact for improved transfer resistance. They also have high tarnish resistance and are suitable for many sensitive, low voltage applications.

Information provided by CMW Inc.

Available Properties
  • Density
  • Hardness, Rockwell 15T
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Electrical Resistivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。