CMW ELKONIUM® 43 palladium based alloy
Subcategory: Precious Metal; Nonferrous Metal; Palladium Alloy
Material Notes: Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting point (1552(C) and, like platinum, resists arc formation. Its low electrical conductivity (16% IACS) limits its application to low current circuits. It costs much less than platinum, and is used as a lower cost alternative. Economics normally dictate that it be supplied as a composite contact with a thin contact metal facing silver brazed to a nickel-plated steel rivet, screw, or projection weld button backing. ELKONIUM® 43 is CMW's trademark for a palladium-silver-copper-nickel alloy having high tensile strength and good resistance to mechanical wear. It is more resistant to sulfide tarnish than fine silver but is susceptible to oxidation at high temperatures and under arcing conditions. It is used as a combination spring and contact in sliding Applications such as potentiometers and instrument commutators. Information provided by CMW Inc.
| Available Properties |
- Density
- Hardness, Rockwell 15T
- Tensile Strength, Ultimate
- Elongation at Break
- Electrical Resistivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|