CMW ELKONITE® 10W53 (Heat Treatable Copper Tungsten)
Subcategory: Metal Matrix Composite; Copper Alloy; Tungsten Alloy; Nonferrous Metal
Material Notes: Uses: Resistance / projection welding electrodes Information provided by CMW Inc.
| Available Properties |
- Density
- Hardness, Rockwell B
- Flexural Modulus
- Electrical Resistivity
- Thermal Conductivity
- Melting Point
- Liquidus
|
|
|
|