CMW ELKONITE® 20S (Infiltrated Tungsten Silver Contact Material) ASTM B531, Class A, infiltrated
Subcategory: Metal Matrix Composite; Silver Alloy; Tungsten Alloy; Nonferrous Metal
Material Notes: For electrical constacts resistant to arcing and welding in circuit breakers, etc. Information provided by CMW Inc.
| Available Properties |
- Density
- Hardness, Rockwell B
- Flexural Modulus
- Electrical Resistivity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |