CMW ELKONITE® 30W3 (Infiltrated Copper Tungsten contact material) ASTM B702, Class E, infiltrated, RWMA Class 12
Subcategory: Metal Matrix Composite; Copper Alloy; Tungsten Alloy; Nonferrous Metal
Material Notes: Foo projection welding dies, die facing, and resistance welding electrodes. Also used for low expansion structural members. Information provided by CMW Inc.
| Available Properties |
- Density
- Hardness, Rockwell B
- Flexural Modulus
- Electrical Resistivity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|