CMW THERMKON® 70M (Molybdenum Copper parts)
  Subcategory: Metal Matrix Composite; Copper Alloy; Nonferrous Metal; Molybdenum Alloy 
Material Notes:  For matching CTE of semiconductor substrates while allowing high thermal transfer. Information provided by CMW Inc. 
  
  
    | Available Properties | 
   
    
    - Density
 
- Hardness, Rockwell B
 
- Tensile Strength, Ultimate
 
- Tensile Strength, Yield
 
- Modulus of Elasticity
 
- Flexural Modulus
 
- Electrical Resistivity
 
- CTE, linear 20°C
 
- Specific Heat Capacity
 
- Thermal Conductivity
 
- Melting Point
 
- Solidus
 
- Liquidus
 
 
   |   
   |   
 | 
   | 
  
  