Cronite 34Ni/25Cr/Nb Nickel Alloy Castings, (Cronite No. HR 33 Nb)
Subcategory: Superalloy; Nickel Alloy; Nickel Base
Close Analogs: Composition Notes: Iron content calculated as remainder.
Key Words: Werkstoff 1.4852
Material Notes: High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries. Information provided by AFE Technologies/North American Cronite, Inc.
|
|
|