Crucible CPM® 3V® Tool Steel
Subcategory: Tool Steel; Metal
Close Analogs: Composition: Iron content calculated as remainder
Material Notes: CPM 3V is a new tool steel made by the Crucible Particle Metallurgy process, designed to provide maximum resistance to breakage and chipping in a highly wear-resistant steel. CPM 3V offers impact toughness greater than A2, D2, Cru-Wear or CPM M4, approaching the levels of S7 and other shock resistant grades, while providing excellent wear resistance, high hardness and thermal stability for coatings. Intended to be used at HRC 58-60 CPM 3V can replace high alloy tool steels in wear applications where chronic tool breakage and chipping problems are encountered. The CPM process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes. Information provided by Crucible Specialty Metals.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Charpy Impact
- CTE, linear 250°C
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|