Crucible CPM®, High Speed Steel Rex® T15(HS)
Subcategory: Tool Steel; High Carbon Steel; Metal
Close Analogs: Composition: Iron content calculated as remainder
Key Words: AISI T15 High Speed Steel
Material Notes: CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobalt for good red hardness. CPM Rex T15 is ideal for cutting difficult to machine materials where high frictional heating is encountered.The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimensional stability, grindability and toughness when compared to steels produced by conventional processes. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking. Information provided by Crucible Specialty Metals.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Flexural Strength
- Charpy Impact
- CTE, linear 250°C
- CTE, linear 500°C
- Shrinkage
- Grindability; Metal Removed/Wheel Worn
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|