Crucible Cru-Wear® Tool Steel

 

Subcategory: Tool Steel; Air-Hardening Steel; High Carbon Steel; Metal

Close Analogs:

Composition:
Iron content calculated as remainder

Material Notes:
CRU-WEAR is an air-hardening tool steel, heat treatable to HRC 60-65. Designed as an upgrade to D2, it offers better wear resistance, greater toughness and higher attainable hardness. Compared to the chemistry of D2, (D2 = 1.55% carbon, 11.5% chromium, 0.8% vanadium, and 0.9% molybdenum), CRU-WEAR has less carbon and less chromium, but more vanadium and tungsten. Both D2 and CRU-WEAR contain carbides for wear resistance, but CRU-WEAR has more vanadium carbides than D2. Vanadium carbides are harder than chromium carbides and are much more effective in providing wear resistance. Because CRU-WEAR contains less carbon than D2, its overall carbide volume is lower, making it tougher than D2. (Note: Although CRU-WEAR contains fewer total carbides, it has more of the type of carbides that are most effective for wear resistance.) CRU-WEAR’s higher attainable hardness results from the fact that it contains sufficient tungsten and molybdenum to cause a secondary hardening response, (up to HRC 65), which does not occur in D2. Finally, CRU-WEAR tempers at a higher range (900-1050°F) than D2 (400-600°F), so it is more compatible with a wide variety of surface treatments.

Information provided by Specialty Metals.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Charpy Impact
  • CTE, linear 250°C
  • Thermal Conductivity
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。