Crucible AIRDI® 150 (AISI D2) Tool Steel
Subcategory: Air-Hardening Steel; High Carbon Steel; Metal
Close Analogs: Composition: Iron content calculated as remainder
Material Notes: Airdi 150 (AISI D2) is an air-hardening, high carbon, high chromium tool steel, heat treatable to HRC 60-62. It offers excellent abrasion resistance, due to a large volume of carbides in the microstructure. Airdi 150 (D2) has been widely used for many years in cold work applications requiring very high wear resistance. It is machinable in the annealed condition and, like other air-hardening tool steels, exhibits minimal distortion on hardening.Information provided by Crucible Specialty Metals.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Charpy Impact
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|