Crucible Nu-Die® V (AISI H13) Hot Work Tool Steel
Subcategory: Tool Steel; Hot Work Steel; Low Carbon Steel; Metal
Close Analogs: Composition: Iron content calculated as remainder
Material Notes: Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and temper resistance, along with moderate wear resistance. It is air hardenable and is used in most applications in the heat treated condition at HRC 44-52. The normal tempering temperatures for Nu-Die V are quite high (>1000°F, 540°C), allowing it to retain its heat treated hardness and strength while in service at elevated temperatures. Nu-Die V may be used for tool temperatures up to about 1000°F (540°C) with brief exposures up to 1100°F (595°C), making it ideal for forging dies, hot extrusion tooling, and die casting dies. Crucible offers two premium versions, Nu-Die XL and Nu-Die ESR, for applications requiring critical polishability, improved heat check resistance and better transverse toughness.Information provided by Crucible Specialty Metals.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Charpy Impact
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|