Crucible AIRKOOL® (AISI A2) Tool Steel

 

Subcategory: Tool Steel; Air-Hardening Steel; Medium Alloy Steel; Metal

Close Analogs:

Composition:
Iron content calculated as remainder

Material Notes:
Airkool (AISI A2) is an air-hardening medium alloy tool steel which is heat treatable to HRC 60-62. It has wear resistance intermediate between the oil hardening tool steels (O1) and the high carbon chromium tool steels (D2). Because it offers a combination of good toughness along with moderate wear resistance, it has been widely used for many years in variety of cold work applications which require fairly high abrasion resistance but where the higher carbon/ high chromium steels are prone to chipping and cracking. Airkool is quite easily machined in the annealed condition and, like other air-hardening tool steels, exhibits minimal distortion on hardening, making it an excellent choice for dies of complicated design.

Information provided by Crucible Specialty Metals.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Charpy Impact
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Thermal Conductivity
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。