Crucible S7 XL (Premium AISI S7) Tool Steel

 

Subcategory: Tool Steel; Mold Steel; Metal

Close Analogs:

Composition:
Iron content calculated as remainder

Material Notes:
Crucible S7XL is a double refined, high purity grade of S7. The remelt operation produces a cleaner steel with a more uniform microstructure, offering the following advantages over conventional S7:

  • Better Consistency in Wire EDM Cutting
  • Higher Polishability for Critical Finish Plastic Molds
  • More Uniform Texturing for Plastic Molds
  • Higher Transverse Impact Toughness (Across the Grain) Crucible S7 XL can be used in any application where AISI S7 is used.

    Information provided by Crucible Specialty Metals.

    Available Properties
    • Density
    • Hardness, Brinell
    • Hardness, Rockwell C
    • Modulus of Elasticity
    • Charpy Impact
    • CTE, linear 250°C
    • CTE, linear 500°C
    • Thermal Conductivity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。