Crucible 430F Stainless Steel
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Low Carbon Steel; Metal; Ferritic
Close Analogs: Composition: Iron content calculated as remainder
Material Notes: Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive enviroments. The chemistry is closely controlled to develop optimum machining and magnetic properties. Information provided by Crucible Specialty Metals.
| Available Properties |
- Specific Gravity
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Reduction of Area
- Fatigue Strength
- Electrical Resistivity
- CTE, linear, 212°F (100°C)
- CTE, linear, 482°F (250°C)
- Thermal Conductivity
- Melting Point
- Endurance Limit, ksi
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|