Crucible 431 Chromium Steel

 

Subcategory: T 400 Series Stainless Steel; Stainless Steel; Low Carbon Steel; Metal

Close Analogs:

Composition:
Iron content calculated as remainder

Material Notes:
Crucible 431 is a nickel bearing chromium steel which can be treated to exeptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar martensitic types. This grade is ferro-magnetic when annealed or heat treated. Because it is characteristically a two phase alloy, the normal structurecontains ferrite and martensite. However depending upon application, the chemistry can be balanced to provide an essentially ferrite-free structure and higher mechanical properties.

Information provided by Crucible Specialty Metals.

Available Properties
  • Specific Gravity
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Reduction of Area
  • Modulus of Elasticity
  • Izod Impact Unnotched
  • Electrical Resistivity
  • CTE, linear, 212°F (100°C)
  • CTE, linear, 482°F (250°C)
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。