Crucible 15-5 Precipitation Hardening Stainless Steel
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Low Carbon Steel; Metal; Martensitic
Close Analogs: Composition: Iron content calculated as remainder
Material Notes: Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness leels after a relatively simple heat-treatment procedure. This grade is a Vacuum Arc remelted for improved cleanliness. Crucible 15-5 is martensitic and magnetic in both the solution-treated and precipitation hardened conditions. It has a high resistance to crack propagation, good transverse properties, and corrosion resistance is normally superior to the regular martensitic chromium-type stainless steels. Because of the single low-temperature(900-1150°F) precipitation-hardening heat treatment of this grade, scaling and distortion are virtually eliminated. This enables material to be finish machined to close tolerances prior to heat treatment. Information provided by Crucible Specialty Metals.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Reduction of Area
- Rupture Strength
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear, 212°F (100°C)
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|