Crucible 15-5 Precipitation Hardening Stainless Steel

 

Subcategory: Stainless Steel; Precipitation Hardening Stainless; Low Carbon Steel; Metal; Martensitic

Close Analogs:

Composition:
Iron content calculated as remainder

Material Notes:
Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness leels after a relatively simple heat-treatment procedure. This grade is a Vacuum Arc remelted for improved cleanliness. Crucible 15-5 is martensitic and magnetic in both the solution-treated and precipitation hardened conditions. It has a high resistance to crack propagation, good transverse properties, and corrosion resistance is normally superior to the regular martensitic chromium-type stainless steels.

Because of the single low-temperature(900-1150°F) precipitation-hardening heat treatment of this grade, scaling and distortion are virtually eliminated. This enables material to be finish machined to close tolerances prior to heat treatment.

Information provided by Crucible Specialty Metals.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break at Elevated Temperature
  • Elongation at Yield
  • Reduction of Area
  • Rupture Strength
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear, 212°F (100°C)
  • CTE, linear, 482°F (250°C)
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。