Crucible 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Low Carbon Steel; Metal; Martensitic
Close Analogs: Composition: Iron content calculated as remainder
Material Notes: Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. The machinability improvement, of up to 45% over conventional solution-treated ( Condition A) 17Cr-4Ni material, has been achieved by close control of the chemical composition within the standard range. Crucible 17Cr-4Ni shows a significant improvement in ductility in all conditions, especially the solution-treated condition. In addition, the steel is markedly tougher than conventional 17Cr-4Ni as measured by Charpy impact tests. Crucible 17Cr-4Ni Super-X is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relativly simple heat-treatment procedure. This grade is martensitic and magnetic in both the solution-treated and precipitation-hardened conditions. It has high resistance to crack propagation, good transverse properties, and corrosion resistance is normally superior to the regular martensitic chromium-type of stainless steel. Because of the single low-temperature (900-1150°F) precipitation-hardening heat treatment of this grade, scaling and distortion are virtually eliminated. This enables materials to be finish machined to close tolerance prior to heat treatment. Information provided by Crucible Specialty Metals.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Reduction of Area
- Rupture Strength
- Modulus of Elasticity
- Charpy Impact
- Fatigue Strength
- Electrical Resistivity
- CTE, linear, 212°F (100°C)
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|