Crucible Compaction Metals P/M Rene 95 Nickel Based Superalloy

 

Subcategory: Superalloy; Nickel Alloy; Nickel Base

Close Analogs:

Composition:
Nickel content calculated as balance.

Key Words: Powder Metallurgy

Material Notes:
P/M Rene 95 is one of the highest strength alloys available for service in the range of 800°F to 1200°F (425°C to 650°C). The alloy also provides excellent high temperature creep resistance and low cycle fatigue life. Tens of thousands of high pressure turbine discs and turbine blades retainers made from Crucible Rene 95 are in service on commercial and military airplanes and helicopters worldwide.

Rene 95 is available as either as-HIP preforms or extruded billet. As-HIP parts can range up to 46 inches (1.2 m) in diameter and weighs up to 16,000 lb (7,200 kg). Extruded billet up to 12 inches (.3 m) in diameter is produced from compacts containing up to 8,000 lb (3,600 kg) of powder.

Advantages:

  • High Strength
  • Excellent high temperature creep resistance
  • Extended low cycle fatigue life

Information provided by Crucible Compaction Metals.

Available Properties
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Reduction of Area
  • Creep Strength
  • Rupture Strength
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。