Crucible Compaction Metals P/M Rene 95 Nickel Based Superalloy
Subcategory: Superalloy; Nickel Alloy; Nickel Base
Close Analogs: Composition: Nickel content calculated as balance.
Key Words: Powder Metallurgy
Material Notes: P/M Rene 95 is one of the highest strength alloys available for service in the range of 800°F to 1200°F (425°C to 650°C). The alloy also provides excellent high temperature creep resistance and low cycle fatigue life. Tens of thousands of high pressure turbine discs and turbine blades retainers made from Crucible Rene 95 are in service on commercial and military airplanes and helicopters worldwide. Rene 95 is available as either as-HIP preforms or extruded billet. As-HIP parts can range up to 46 inches (1.2 m) in diameter and weighs up to 16,000 lb (7,200 kg). Extruded billet up to 12 inches (.3 m) in diameter is produced from compacts containing up to 8,000 lb (3,600 kg) of powder. Advantages: - High Strength
- Excellent high temperature creep resistance
- Extended low cycle fatigue life
Information provided by Crucible Compaction Metals.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Reduction of Area
- Creep Strength
- Rupture Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|