Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy

 

Subcategory: Superalloy; Nickel Alloy; Nickel Base

Close Analogs:

Composition:
Nickel content calculated as balance.

Key Words: UNS N06625; Powder Metallurgy

Material Notes:
P/M 625 (chemically, UNS N06625) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The advanced Crucible powder consolidation operation guarantees a fully dense, fine grained product. Crucible custom crafted parts can be machined in less time and with less tool wear than those produced from conventional 625 material.

P/M 625 gives engineers and designers great flexibility in design. It is available in standard mill forms such as billet, bar, and tubing, and as near net shapes and clad components and hollows. The use of near net shapes can decrease the amount of material used and drastically cut the costs of fabricating a finished part.

Suggested Processing Conditions: Q & T - Water Quench at 996°C for 1 hour and Air Cool at 677°C for 6 hours; Double Age - Furnace Cool at 718°C for 8 hours and Air Cool from 38°C to 622°C for 8 hours.; ST&A4 - Water Quench at 982°C for 1 hour and Air Cool at 649°C for 16 hours; As-HIP: As-Hot Isostatic Pressed

Advantages:

  • Near net shape
  • Excellent corrosion resistance
  • Heat treatment for superior strength
  • Flexibility in design

Information provided by Crucible Compaction Metals.

Available Properties
  • Environmental Stress Crack Resistance
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Charpy Impact
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。