Crucible Compaction Metals P/M 625M Corrosion Resistant Alloy

 

Subcategory: Superalloy; Nickel Alloy; Nickel Base

Close Analogs:

Composition:
Nickel content calculated as balance.

Key Words: UNS N07626; Powder Metallurgy

Material Notes:
P/M 625M (chemically, UNS N07626) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The advanced Crucible powder consolidation operation guarantees a fully dense, fine grained product. Crucible custom crafted parts can be produced with shorter lead times and less user costs than comparable conventional alloys.

Crucible P/M 625M is a patented composition designed to take advantage of the aging response associated with rapid solidification rate powder metallurgy technology. Those elements (Al, Cb, and Ti) which effect the precipitation reactions have been optimized to achieve yield strengths above 120 ksi. The rest of the composition has been balanced to maintain good corrosion resistance. P/M 625M offers both a high strength level, like that of alloy 718, and good corrosion resistance, like that of Crucible P/M 625, in one alloy. Engineers and designers no longer have to choose one or the other. Since Crucible produces this alloy by powder metal techniques, lower total costs are a reality. If material is purchased as a near net shape or a clad product, less weight has to be bought. This makes fabrication easier and significantly lowers over manufacturing cost.

Advantages:

  • Near new shapes
  • Fastener material
  • Excellent corrosion resistance
  • Excellent strength
  • Flexibility in design
  • NACE MR-01-75 approved

Information provided by Crucible Compaction Metals.

Available Properties
  • Environmental Stress Crack Resistance
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Charpy Impact
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。