Crucible Compaction Metals P/M N625 Corrosion Resistant Alloy
Subcategory: Superalloy; Nickel Alloy; Nickel Base
Close Analogs: Composition: Nickel content calculated as balance.
Key Words: UNS N06625; Powder Metallurgy
Material Notes: P/M N625 (chemically, UNS N06625) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The advanced Crucible powder consolidation operation guarantees a fully dense, fine grained product. Crucible custom crafted parts can be machined in less time and with less tool wear than those produced from conventional 625 material. P/M N625 gives engineers and designers great flexibility in design. It is available in standard mill forms and as billet, bar and tubing, near net shapes and clad components and hollows. The use of near net shapes can decrease the amount of material used and reduces the costs of fabricating a finished part. Advantages: - Near net shape
- Excellent corrosion resistance
- Weldability
- Thermal stability
- Chemical homogeneity
- High strength
- Machinability
Information provided by Crucible Compaction Metals.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|