|   Deloro® alloy 711 PM, P/M, tested at 538°C (1000°F)  Subcategory: Superalloy; Nickel Base Material Notes: Deloro 711 is currently being developed. Nickel content as balance. Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data P/M 6 mm^3, cast 26 mm^3. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts.  Data provided by the manufacturer, Deloro Stellite Inc.
 
| | 
    | Available Properties |  
    | DensityHardness, BrinellHardness, KnoopHardness, Rockwell AHardness, Rockwell BHardness, Rockwell CHardness, VickersTensile Strength, UltimateElongation at Break
 | 
 | 
 |  | | 