Deloro® alloy 40G

 

Subcategory: Superalloy; Nickel Base

Close Analogs: Deloro 40

Material Notes:
Nickel base. Good combination of wear resistance, corrosion resistance, machinability, and repairability. Machined with tungsten carbide tools, using slow speeds and light feeds. Finish grinding achieved with vitrified silicon carbine wheels. Applications include bottle making mold components such as neck rings, half bushings, and die inserts, also used for sealing faces in values in both the oil and nuclear industries. Normally resistant to atmospheric, steams salt water and salt spray corrosion. Excellent oxidation resistance up to melting range. Satisfactory performance in many organic acids but high corrosion rates observed in hot, strong inorganic acids. Highly resistant to semi-molten glass. Normally used in the as-cast condition. Data provided by the manufacturer, Deloro Stellite Inc.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell A
  • Hardness, Rockwell B
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Charpy Impact, Unnotched
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。